以下是BASF PA66 Ultramid A3EG3中英文物性表
| 
						BASF Ultramid? A3EG3 PA66(尼龍66-聚酰胺)
					 
						The property table is provided by www.plas-cn.com, welcome to download, reprint please indicate the source!
					 | |||
| 
						Physical Properties物理性質(zhì)
					 | 
						Metric公制數(shù)據(jù)
					 | 
						English英制數(shù)據(jù)
					 | 
						Comments測(cè)試方法
					 | 
| 
						Density密度 
					 | 
						1.24 g/cc
					 | 
						0.0448 lb/in3
					 | 
						ISO 1183
					 | 
| 
						Water Absorption吸水率 
					 | 
						7.0 %
					 | 
						7.0 %
					 | 
						ISO 62
					 | 
| 
						Moisture Absorption at Equilibrium吸濕平衡 
					 | 
						2.2 %
					 | 
						2.2 %
					 | 
						23°C/50% R.H.; ISO 62
					 | 
| 
						Viscosity Test粘度 
					 | 
						145 cm3/g
					 | 
						145 cm3/g
					 | 
						Viscosity number
					 | 
| 
						Linear Mold Shrinkage線性收縮率 
					 | 
						0.0055 cm/cm
					 | 
						0.0055 in/in
					 | 
						ASTM Data; MD
					 | 
| 
						Melt Flow熔體流動(dòng)速率 
					 | 
						70 g/10 min @Load 11.0 lb, Temperature 527 °F | 
						ISO 1133
					 | |
| 
						Mechanical Properties力學(xué)性能
					 | 
						Metric公制數(shù)據(jù)
					 | 
						English英制數(shù)據(jù)
					 | 
						Comments測(cè)試方法
					 | 
| 
						Tensile Strength at Break斷裂拉伸強(qiáng)度 
					 | 
						114 MPa
					 | 
						16500 psi
					 | 
						0.2 in/min; ASTM Test
					 | 
| 
						156 MPa @Temperature -40.0 °C | 
						22600 psi @Temperature -40.0 °F | 
						ISO Data
					 | |
| 
						Tensile Strength, Ultimate極限拉伸強(qiáng)度 
					 | 
						130 MPa
					 | 
						18900 psi
					 | 
						5mm/min; ISO 527
					 | 
| 
						Tensile Strength, Yield屈服拉伸強(qiáng)度 
					 | 
						74.0 MPa @Temperature 80.0 °C | 
						10700 psi @Temperature 176 °F | 
						ISO Data
					 | 
| 
						Elongation at Break斷裂伸長(zhǎng)率 
					 | 
						3.0 %
					 | 
						3.0 %
					 | 
						5mm/min; ISO 527
					 | 
| 
						3.0 %
					 | 
						3.0 %
					 | 
						0.2 in/min; ASTM Test
					 | |
| 
						2.6 % @Temperature -40.0 °C | 
						2.6 % @Temperature -40.0 °F | 
						ISO Data
					 | |
| 
						Elongation at Yield屈服伸長(zhǎng)率 
					 | 
						7.4 % @Temperature 80.0 °C | 
						7.4 % @Temperature 176 °F | 
						ISO Data
					 | 
| 
						Tensile Modulus拉伸模量 
					 | 
						5.86 GPa
					 | 
						850 ksi
					 | 
						ASTM Test
					 | 
| 
						6.00 GPa
					 | 
						870 ksi
					 | 
						1mm/min; ISO 527
					 | |
| 
						Flexural Strength彎曲強(qiáng)度 
					 | 
						180 MPa
					 | 
						26100 psi
					 | 
						ISO Data
					 | 
| 
						Flexural Modulus彎曲彈性模量 
					 | 
						5.17 GPa
					 | 
						750 ksi
					 | 
						ASTM Test
					 | 
| 
						5.20 GPa
					 | 
						754 ksi
					 | 
						ISO Data
					 | |

 
	

 

 
												 點(diǎn)擊圖片查看大圖
 點(diǎn)擊圖片查看大圖




 免責(zé)聲明:(1)以上所展示的信息由企業(yè)自行提供,內(nèi)容的真實(shí)性、準(zhǔn)確性和合法性由發(fā)布企業(yè)負(fù)責(zé),環(huán)球塑化網(wǎng)對(duì)此不承擔(dān)任何保證責(zé)任。我們?cè)瓌t上建議您優(yōu)先選擇“塑企通”會(huì)員合作! (2)同時(shí)我們鄭重提醒各位買/賣家,交易前請(qǐng)?jiān)敿?xì)核實(shí)對(duì)方身份,切勿隨意打款或發(fā)貨,謹(jǐn)防上當(dāng)受騙。如發(fā)現(xiàn)虛假信息,請(qǐng)向環(huán)球塑化網(wǎng)舉報(bào)。
 免責(zé)聲明:(1)以上所展示的信息由企業(yè)自行提供,內(nèi)容的真實(shí)性、準(zhǔn)確性和合法性由發(fā)布企業(yè)負(fù)責(zé),環(huán)球塑化網(wǎng)對(duì)此不承擔(dān)任何保證責(zé)任。我們?cè)瓌t上建議您優(yōu)先選擇“塑企通”會(huì)員合作! (2)同時(shí)我們鄭重提醒各位買/賣家,交易前請(qǐng)?jiān)敿?xì)核實(shí)對(duì)方身份,切勿隨意打款或發(fā)貨,謹(jǐn)防上當(dāng)受騙。如發(fā)現(xiàn)虛假信息,請(qǐng)向環(huán)球塑化網(wǎng)舉報(bào)。
     簡(jiǎn)繁切換
簡(jiǎn)繁切換