PC S3000R 日本三菱化成工業(yè)公司 物性數(shù)據(jù)
|
|
①原料描述部分
|
|||
|
規(guī)格級(jí)別:
|
---
|
外觀顏色:
|
---
|
|
用途概述:
|
---
|
||
|
備注說(shuō)明:
|
特性:FDA認(rèn)可
|
||
|
②原料技術(shù)數(shù)據(jù)
|
||||||||||||
|
性能項(xiàng)目
|
試驗(yàn)條件[狀態(tài)]
|
測(cè)試方法
|
測(cè)試數(shù)據(jù)
|
數(shù)據(jù)單位
|
||||||||
|
基本性能
|
吸水率
|
23℃,24hr
|
ASTM D-570
|
0.23-0.26
|
%
|
|||||||
|
熔體流動(dòng)速率
|
300℃,1.2kg
|
ISO Standard
|
11-14.5
|
g/10min
|
||||||||
|
物理性能
|
比重
|
---
|
ASTM D-792
|
1.2
|
---
|
|||||||
|
機(jī)械性能
|
拉伸強(qiáng)度
|
23℃
|
ASTM D-638
|
58.8-68.6(600-700)
|
MPa(Kgf/cm2)
|
|||||||
|
拉伸長(zhǎng)度
|
23℃
|
ASTM D-638
|
90-140
|
%
|
||||||||
|
撓曲強(qiáng)度
|
23℃
|
ASTM D-790
|
80-4-90.2(820-920)
|
MPa(Kgf/cm2)
|
||||||||
|
彎曲模度
|
23℃
|
ASTM D-790
|
2.3(2.3)
|
GPa(104Kgf/cm2)
|
||||||||
|
IZOD缺口沖擊強(qiáng)度
|
3.2mm
|
ASTM D-256
|
740-1000(75-102)
|
J/m(Kfg?cm/cm)
|
||||||||
|
洛氏硬度
|
---
|
ASTM D-785
|
R122-124(M60-70)
|
---
|
||||||||
|
電氣性能
|
介電常數(shù)(電容率)
|
106Hz
|
---
|
25.2(2.85)
|
pF/m
|
|||||||
|
介電損耗正切
|
106Hz
|
ASTM D-150
|
0.0082
|
---
|
||||||||
|
表面電阻系數(shù)
|
---
|
ASTM D-257
|
1015
|
---
|
||||||||
|
體積電阻系數(shù)
|
---
|
ASTM D-257
|
2.1×1016
|
cm
|
||||||||
|
耐電壓
|
---
|
ASTM D-149
|
18-22
|
MV/m
|
||||||||
|
加工性能
|
|
---
|
---
|
|
|
|||||||
|
熱 性 能
|
線膨脹系數(shù)
|
20℃-80℃
|
ASTM D-696
|
6-7
|
10-5?K-1
|
|||||||
|
燃燒性
|
1.6mm
|
UL 94
|
HB
|
---
|
||||||||
|
負(fù)荷撓曲溫度
|
455kPa(4.6Kgf/cm2)
|
ASTM D-648
|
136-142
|
℃
|
||||||||
|
負(fù)荷撓曲溫度
|
820kPa(18.6Kgf/cm2)
|
ASTM D-648
|
130-136
|
℃
|
||||||||





簡(jiǎn)繁切換